Material Densification
Technical Publication

Super-Solidus Hot Isostatic Pressing Heat Treatments for Advanced Single Crystal Ni-Base Superalloys

Super-solidus hot isostatic pressing (SSHIP) heat treatment has been developed and applied to CMSX-10 K, a third-generation Ni-base single crystal superalloy. This innovative approach aims to reduce the total time required for solution heat treatment while enhancing mechanical properties compared to conventional routes. SSHIP is suitable for all types of Ni-base single crystal superalloys, particularly those with high refractory element content and a significant volume fraction of eutectic microstructure in the as-cast state.

Share:

Related content

White paper

Reducing heat treatment distortion through High Pressure Heat Treatment (HPHT™)

3D printed Ti6Al4V acetabular cup with delicate trabecular surface structure prone to alpha-case embrittlement
Technical Publication

Meeting demands for manufactured medical implants

Brochure

High-end sinter-based parts powered by Hot Isostatic Pressing

Webinar

Innovations and trends in Hot Isostatic Pressing for orthopedic implants

Customer Stories

Morgan Advanced Materials improves productivity and eliminates scrap with advanced CIP upgrade

Post-Processing Contributions to Fatigue Variability in L-PBF Ti6Al4V with UW
Tech Talks

Post-processing contributions to fatigue variability in L-PBF Ti6Al4V with the University of Washington

Need help choosing the right press for your business?

Do not hesitate to contact us. We are always ready to answer your questions.