Effect of porosity and eutectics on the high-temperature low-cycle fatigue performance of a nickel-base single-crystal superalloy

This study examines the impact of porosity and γ/γ′-eutectics on the low-cycle fatigue life of a single-crystal Ni-based superalloy at high temperatures. Various material variants were produced using different heat treatments, including hot isostatic pressing. Electron microscopy revealed that both pores and γ/γ′-eutectics initiate cracks, leading to early failure. The findings suggest that remaining γ/γ′-eutectics may weaken fatigue resistance more than pores. Additionally, proper integrated hot isostatic pressing heat treatments enhance fatigue performance.

Share:

Related content

White paper

Reducing heat treatment distortion through High Pressure Heat Treatment (HPHT™)

3D printed Ti6Al4V acetabular cup with delicate trabecular surface structure prone to alpha-case embrittlement
Technical Publication

Meeting demands for manufactured medical implants

Brochure

High-end sinter-based parts powered by Hot Isostatic Pressing

Webinar

Innovations and trends in Hot Isostatic Pressing for orthopedic implants

Customer Stories

Morgan Advanced Materials improves productivity and eliminates scrap with advanced CIP upgrade

Post-Processing Contributions to Fatigue Variability in L-PBF Ti6Al4V with UW
Tech Talks

Post-processing contributions to fatigue variability in L-PBF Ti6Al4V with the University of Washington

Need help choosing the right press for your business?

Do not hesitate to contact us. We are always ready to answer your questions.