As-Built and Post-treated Microstructures of an Electron Beam Melting (EBM) Produced Nickel-Based Superalloy

The microstructures of an electron beam melted (EBM) nickel-based superalloy (Alloy 718) were examined in both as-built and post-treated conditions, focusing on the contour and hatch regions of the build. Both regions exhibited similar hardness and carbide content, but the contour region had a higher density of fine carbides. Post-treatments, such as hot isostatic pressing (HIP) and HIP plus heat treatment (HIP + HT), significantly reduced defect content in both regions. Grain coarsening occurred in the contour region after HIP + HT. Various factors contributing to grain growth were discussed, and carbide sizes became more similar after post-treatment. Additionally, both regions showed increased hardness after HIP + HT compared to the as-built material.

Share:

Related content

White paper

Reducing heat treatment distortion through High Pressure Heat Treatment (HPHT™)

3D printed Ti6Al4V acetabular cup with delicate trabecular surface structure prone to alpha-case embrittlement
Technical Publication

Meeting demands for manufactured medical implants

Brochure

High-end sinter-based parts powered by Hot Isostatic Pressing

Webinar

Innovations and trends in Hot Isostatic Pressing for orthopedic implants

Customer Stories

Morgan Advanced Materials improves productivity and eliminates scrap with advanced CIP upgrade

Post-Processing Contributions to Fatigue Variability in L-PBF Ti6Al4V with UW
Tech Talks

Post-processing contributions to fatigue variability in L-PBF Ti6Al4V with the University of Washington

Need help choosing the right press for your business?

Do not hesitate to contact us. We are always ready to answer your questions.